Stainless steel bolts seize because the thread surfaces weld together under pressure. You can lower the risk during assembly, or remove the cause by hardening the thread surface.
You tighten a stainless steel bolt. Halfway down it gets stiff, then it locks. It will not go further and it will not come back out. In the end you cut it off and replace both parts.
That is thread galling. It costs time on the assembly line and it is worse in the field, where a seized bolt can stop a whole installation. On this page you will read:
- What thread galling is and why stainless steel is sensitive to it.
- Which causes you can control during assembly.
- What quick fixes do, and where they stop working.
- How a hardened thread surface prevents galling for good.
What is thread galling?
Thread galling is a form of adhesive wear between the threads of a bolt and a nut. Under pressure and friction, small high points on the two thread surfaces bond. As you keep turning, material tears off one surface and sticks to the other. The damage builds up with every turn until the threads lock.
Galling is also called cold welding or seizing. The names describe the same result: two metal parts that have fused without heat being applied on purpose. Read more about the mechanism on our page about cold welding of stainless steel.
Why do stainless steel bolts and nuts seize so easily?
Stainless steel resists corrosion because of a very thin oxide layer on its surface. That layer is what makes the material useful, and it is also the weak point in a threaded connection.
When you tighten a fastener, the thread flanks slide over each other under high pressure. The oxide layer is wiped away faster than it can form again. Bare metal now touches bare metal. The common austenitic grades, such as 304 and 316, are relatively soft and ductile, so the exposed surfaces bond easily.
Other metals that protect themselves with an oxide layer, such as aluminum and titanium, show the same behavior.
Which causes of thread galling can you control?
Galling starts with the material, but assembly conditions decide whether it happens. These are the factors you can influence:
- Tightening speed. Power tools build up friction heat quickly, and stainless steel does not conduct heat away well. Slower tightening lowers the risk.
- Thread condition. Rough, damaged or dirty threads have more high points that can bond. Clean, smooth threads gall less.
- Identical materials. A bolt and nut of the same grade and the same hardness are the most sensitive combination.
- Load during tightening. Using the bolt to pull parts together, or tightening at an angle, raises the pressure on the thread flanks.
- Dry assembly. Without a lubricating film the surfaces are in direct contact from the first turn.
What do the quick fixes do, and where do they stop?
Most advice on thread galling is about assembly. These measures help, and each has a limit.
| Measure | What it does | Where it stops |
|---|---|---|
| Lubricant or anti-seize paste | Separates the surfaces and lowers friction | Often not allowed in food, pharma or cleanroom equipment; must be reapplied at every assembly; changes the torque you need |
| Tightening slowly, by hand if needed | Less friction heat | Depends on the person and the time available |
| Different grades for bolt and nut | Creates a hardness difference | The difference between common grades is small and not always enough |
| Cleaning and inspecting threads | Removes dirt and damaged spots | Does not change the material itself |
These measures lower the chance of galling. They do not remove the cause, which is two soft stainless steel surfaces sliding over each other. For connections that are opened and closed often, or where lubricant is not an option, that is not enough.
How do you prevent thread galling permanently?
The lasting solution is to make the thread surface harder. A hard surface does not deform and bond the way untreated stainless steel does, so the threads keep sliding instead of tearing.
Stainihard® is a surface hardening process for stainless steel from Aalberts Surface Technologies. It is not a coating, so there is no layer that can flake or wear through. According to Aalberts Surface Technologies, the process counters cold welding while the corrosion resistance of the stainless steel is maintained. Treating one of the two parts, the bolt or the nut, is usually enough to prevent the connection from seizing.
Read how stainless steel hardening works and which materials are suitable.
Are your stainless steel connections seizing?
Tell us which parts are involved, which grade they are made of and how often the connection is opened. Our engineers will tell you whether treatment makes sense for your application.
When does treating fasteners pay off?
Treatment is worth considering when one of these applies:
- The connection is assembled and disassembled regularly, for example for cleaning or maintenance.
- Lubricants are not allowed or are washed away, as in food processing and pharmaceutical equipment.
- A seized fastener means downtime or damage to an expensive component.
- The fasteners are hard to reach once the equipment is installed.
See more examples of applications.
Frequently asked questions about thread galling
Yes. Thread galling is cold welding that takes place in a threaded connection. Galling is the term engineers use most; cold welding and seizing describe the same effect.
Usually not without damage. Once the threads have bonded, turning further tears more material loose. In most cases the bolt has to be cut or drilled out and both parts replaced.
No. Aluminum and titanium fasteners gall as well. Stainless steel is the most common case because it is used so widely for bolts and nuts.
It lowers the risk as long as it is applied correctly at every assembly. It is not a solution where lubricants are not permitted, and it changes the relationship between torque and clamping force, so the tightening torque has to be adjusted.
Treating one of the two parts is usually sufficient, because the hardened surface no longer bonds with the untreated one.